At present, domestic high-end casting products have increasingly strict requirements for harmful components such as titanium, phosphorus, manganese, and vanadium in pig iron. However, in the smelting process, the technology for removing titanium, phosphorus, and vanadium is not yet mature. The key to reducing the titanium, phosphorus, and vanadium content in ductile iron lies in selecting high-quality iron concentrate powder, optimizing the ingredients, and smelting. LG brand ductile iron uses high-quality iron ore from local and adjacent counties as the main raw material, using ultra-low furnace temperature smelting, constant silicon addition outside the furnace, and other technologies to ensure that the titanium, phosphorus, and vanadium content in the iron ball is effectively controlled within 0.03, the manganese content is within 0.1, and the arsenic content is within 0.0005, The chromium content should be within 0.05, and the vanadium content should be controlled within 0.01.
At present, domestic high-end casting products have increasingly strict requirements for harmful components such as titanium, phosphorus, manganese, and vanadium in pig iron. However, in the smelting process, the technology for removing titanium, phosphorus, and vanadium is not yet mature. The key to reducing the titanium, phosphorus, and vanadium content in ductile iron lies in selecting high-quality iron concentrate powder, optimizing the ingredients, and smelting. LG brand ductile iron uses high-quality iron ore from local and adjacent counties as the main raw material, using ultra-low furnace temperature smelting, constant silicon addition outside the furnace, and other technologies to ensure that the titanium, phosphorus, and vanadium content in the iron ball is effectively controlled within 0.03, the manganese content is within 0.1, and the arsenic content is within 0.0005, The chromium content should be within 0.05, and the vanadium content should be controlled within 0.01.
Product Series |
Mark |
Composition standards(%) |
|||||
Si |
Ti |
Mn |
P |
S |
C |
||
Ductile castiron |
特Q6 |
0.5-0.60 |
≤0.030 |
≤0.150 |
≤0.035 |
≤0.020 |
≥3.40 |
特Q7 |
0.61-0.70 |
≤0.035 |
≤0.150 |
≤0.035 |
≤0.020 |
||
特Q8 |
0.71-0.80 |
≤0.035 |
≤0.150 |
≤0.035 |
≤0.020 |
||
特Q9 |
0.81-0.90 |
≤0.038 |
≤0.150 |
≤0.035 |
≤0.020 |
||
特Q10 |
0.91-1.00 |
≤0.040 |
≤0.150 |
≤0.035 |
≤0.020 |
||
一级Q6 |
0.50-0.60 |
≤0.040 |
0.15-0.20 |
≤0.040 |
≤0.020 |
≥3.4 |
|
一级Q7 |
0.61-0.70 |
≤0.040 |
0.15-0.20 |
≤0.040 |
≤0.020 |
||
一级Q8 |
0.71-0.80 |
≤0.040 |
0.15-0.20 |
≤0.040 |
≤0.020 |
||
一级Q9 |
0.81-0.90 |
≤0.040 |
0.15-0.20 |
≤0.040 |
≤0.020 |
||
一级Q10 |
0.91-1.00 |
≤0.040 |
0.15-0.20 |
≤0.040 |
≤0.020 |
||
特Q12 |
1.01-1.2 |
≤0.050 |
≤0.040 |
≤0.020 |
≥3.4 |
||
特Q14 |
1.21-1.40 |
≤0.050 |
≤0.040 |
≤0.020 |
≥3.4 |
||
特Q16 |
1.41-1.60 |
≤0.050 |
≤0.040 |
≤0.020 |
|||
特Q18 |
1.61-1.8 |
≤0.055 |
≤0.040 |
≤0.020 |
|||
二级Q6 |
0.50-0.60 |
≤0.050 |
≤0.040 |
≤0.030 |
≥3.40 |
||
二级Q7 |
0.61-0.70 |
≤0.050 |
≤0.040 |
≤0.030 |
|||
二级Q8 |
0.71-0.80 |
≤0.050 |
≤0.040 |
≤0.030 |
|||
二级Q9 |
0.81-0.90 |
≤0.050 |
≤0.040 |
≤0.030 |
|||
二级Q10 |
0.91-1.00 |
≤0.050 |
≤0.040 |
≤0.030 |
|||
二级Q12 |
1.01-1.20 |
≤0.050 |
≤0.040 |
≤0.030 |
|||
二级Q14 |
1.21-1.40 |
≤0.050 |
≤0.040 |
≤0.030 |